3/29/2024 | 8108905008 | MECHANICALLY PROCESSED TI-6AL-4V TITANIUM ALLOY PLATES FROM MELTS 8-11-12135-2 8-23-08351 8-31-08794 8-46-12928 ARE PRODUCED BY FORGING AND ROLLING BLANKS OBTAINED BY ELECTRIC VACUUM REMELT. PURPOSE - CIVIL AIRCRAFT ENGINEERING. | XXXXXXXXXX | 1 | N/A | 238696.53 | France | OBERTSHAUSEN |
3/29/2024 | 8108905008 | MACHINED PLATES AND SHEETS ACCORDING TO AMS 4911 SPECIFICATIONS FROM TITANIUM ALLOYS TI6AL4V. FROM HEATS 8-09-11364 8-09-11373 8-17-10576 8-18-09867 8-21-08676 8-21-08688 WITH ULTRA-STRENGTH GREATER THAN 930 MPa. MADE BY ROLLING BLANKS, | XXXXXXXXXX | 1 | N/A | 385481.73 | Spain | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED SHEETS AND PLATES ACCORDING TO SPECIFICATIONS WL 3.7164.1 DIN 65039 LN 9297 MADE OF TITANIUM ALLOY 3.7164.1 FROM MELT 8-22-07981 8-46-12875 TENSILE STRENGTH MORE THAN 930 MPa. MADE BY ROLLING BLANKS OBTAINED BY ELECTRIC VACUUM | XXXXXXXXXX | 1 | N/A | 52153.64 | Turkey | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED PLATES, MADE TO SPECIFICATION ABS 5125, AIMS 03-18-006, IPS 03-18-006-05 FROM TITANIUM ALLOY TI6AL-4V. MELT 8-21-08702. TENSILE STRENGTH NOT LESS THAN 930 MPa. MADE BY ROLLING BLANKS OBTAINED | XXXXXXXXXX | 1 | N/A | 60161.93 | France | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED SHEETS, MADE TO SPECIFICATION ABS 5326C, AIMS 03-18-004. FROM TITANIUM ALLOY TI6AL4V. MELT 8-21-08654. TENSILE STRENGTH MPa - NOT LESS THAN 930. MADE BY ROLLING BLANKS OBTAINED BY ELECTRIC VACUUM REMELT. | XXXXXXXXXX | 1 | N/A | 46198.81 | France | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED SHEETS ACCORDING TO SPECIFICATION ABS 5326 AIMS 03-18-004 MADE OF TITANIUM ALLOY TI6AL4V - 8 PCS: SIZE 1.4/1250/2500 MM: FROM MELT 8-03-09554 TENSILE STRENGTH MORE THAN 930 MPa: MADE BY ROLLING BLANKS OBTAINED BY ELECTRIC VACUUM | XXXXXXXXXX | 1 | N/A | 9928.39 | Turkey | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED PLATES, MADE TO SPECIFICATION ABS 5125, FROM TITANIUM ALLOY TI6AL4V. MELT 8-36-12062. STRENGTH ULTRA-STRENGTH MPa - NOT LESS THAN 930, MADE BY ROLLING BLANKS OBTAINED BY ELECTRIC VACUUM REMELT. PURPOSE - | XXXXXXXXXX | 1 | N/A | 16269.25 | United Kingdom | REDDITCH |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED PLATES ACCORDING TO SPECIFICATION ABS 5125 FROM TITANIUM ALLOY TI6AL4V(GR5), MELT 8-22-07981,8-04-11488. STRENGTH ULTRA-STRENGTH MPA - MORE THAN 930. MADE BY ROLLING BLANKS OBTAINED BY ELECTRIC VACUUM REMELT. | XXXXXXXXXX | 1 | N/A | 16590.1 | France | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED TI6AL4V TITANIUM ALLOY PLATES FROM 8-02-06494 MELTS, STRENGTH MORE THAN 930 MPa. MADE BY ROLLING BLANKS OBTAINED BY ELECTRO-VACUUM REMELT. PURPOSE - CIVIL AIRCRAFT ENGINEERING. | XXXXXXXXXX | 1 | N/A | 69766.46 | Germany | OBERTSHAUSEN |
3/28/2024 | 8108905008 | MECHANICALLY PROCESSED SHEETS, MADE TO SPECIFICATION ABS 5326, AIMS 03-18-004, LN 9297, DIN 65039, FROM TITANIUM ALLOY 3.7164.1, TI-6AL-4V. HEAT 8-41-12788, 8-17-10629, 8-45-12892. THE ULTIMATE STRENGTH IS NOT LESS THAN 930 MPa. MADE BY THE METHOD | XXXXXXXXXX | 1 | N/A | 23912.57 | France | OBERTSHAUSEN |