3/12/2024 | 7601208009 | ALUMINIUM ALLOY IN THE FORM OF A SMALL-SIZED IRON CONTAINING LESS THAN 99.0% ALUMINUM, 36 CONTAINERS, METAL FIXED WITH WOODEN PROPS. TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR B | XXXXXXXXXX | 1 | N/A | 61349852.55 | India | GONCHAROVO |
3/11/2024 | 7601208009 | ALUMINUM ALLOY IN THE FORM OF A SMALL-SIZED INK CONTAINING LESS THAN 99.0% ALUMINUM, 21 CONTAINERS, METAL FIXED WITH WOODEN PROPS. TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR HIGHER | XXXXXXXXXX | 2 | N/A | 97495289.94 | India | DIFFERENT |
3/11/2024 | 7601208009 | ALUMINIUM ALLOY IN THE FORM OF A SMALL-SIZED IRON CONTAINING LESS THAN 99.0% ALUMINUM, 10 CONTAINERS, METAL FIXED WITH WOODEN PROPS. TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR B | XXXXXXXXXX | 2 | N/A | 47625057.81 | India | DIFFERENT |
3/11/2024 | 7601208009 | ALUMINIUM ALLOY IN THE FORM OF A SMALL-SIZED IRON CONTAINING LESS THAN 99.0% ALUMINUM, 27 CONTAINERS, METAL FIXED WITH WOODEN PROPS. TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR B | XXXXXXXXXX | 2 | N/A | 125490670.84 | India | DIFFERENT |
3/5/2024 | 7601208009 | ALUMINUM ALLOY IN THE FORM OF A SMALL-SIZED INK CONTAINING LESS THAN 99.0% ALUMINUM, 6 CONTAINERS, METAL FIXED WITH WOODEN PROPS, TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR YOU | XXXXXXXXXX | 2 | N/A | 26765751.34 | India | DIFFERENT |
3/5/2024 | 7601208009 | ALUMINIUM ALLOY IN SMALL-SIZED IRON FORM CONTAINING LESS THAN 99.0% ALUMINUM, 25 CONTAINERS, METAL FIXED WITH WOODEN PROPS. TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR IN | XXXXXXXXXX | 2 | N/A | 100617452.71 | India | DIFFERENT |
3/5/2024 | 7601208009 | ALUMINIUM ALLOY IN THE FORM OF A SMALL-SIZED IRON CONTAINING LESS THAN 99.0% ALUMINUM, 48 CONTAINERS, METAL FIXED WITH WOODEN PROPS: TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR IN | XXXXXXXXXX | 2 | N/A | 180810849.09 | India | DIFFERENT |
2/27/2024 | 7601208009 | ALUMINUM ALLOY IN THE FORM OF A SMALL-SIZED INK CONTAINING LESS THAN 99.0% ALUMINUM, 36 CONTAINERS, THE METAL IS FIXED WITH A WOODEN PROP. THE TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR YOU | XXXXXXXXXX | 0 | N/A | 155580857.2 | India | DIFFERENT |
2/19/2024 | 7601208009 | ALUMINUM ALLOY IN THE FORM OF A SMALL-SIZED INK CONTAINING LESS THAN 99.0% ALUMINUM, THE METAL IS FIXED WITH A WOODEN PROP. THE TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR HIGHER AT A TEMPERATURE OF | XXXXXXXXXX | 0 | N/A | 94573760.92 | India | BATTERY |
2/19/2024 | 7601208009 | ALUMINUM ALLOY IN THE FORM OF A SMALL-SIZED INK CONTAINING LESS THAN 99.0% ALUMINUM, THE METAL IS FIXED WITH A WOODEN PROP. THE TENSILE STRENGTH DOES NOT REACH 240 MPa OR HIGHER AT A TEMPERATURE OF 473 K (200 DEG C) OR 415 MPa OR HIGHER AT A TEMPERATURE OF | XXXXXXXXXX | 0 | N/A | 99718364.98 | India | GONCHAROVO |