3/14/2024 | 7601208002 | ALUMINUM ALLOYS SECONDARY UNPROCESSED IN INGOTS IN THE FORM OF PIECES OF SIZE 695-645X70-100X45MM GRADE ADC12 ACCORDING TO STANDARD JIS H 5302-2006 WITH ULTIMATE TENSILE STRENGTH LESS THAN 216 MPa AT TEMPERATURE OF 298 K FOR USE IN METALLURGY | XXXXXXXXXX | 1 | N/A | 401012.02 | China | NINGBO |
3/12/2024 | 7601208002 | SECONDARY ALUMINUM ALLOYS IN PIECES, OBTAINED BY RE-MELTING ALUMINUM WASTE AND SCRAP, GRADE DIN226, TU 24.42.11-001-52271102-2020. TENSILE STRENGTH LESS THAN 240 MPa AT 200 GREEN C AND LESS THAN 415 MPa AT 25 GREEN C. | XXXXXXXXXX | 1 | N/A | 473389.42 | China | EKATERINBURG |
3/6/2024 | 7601208002 | ALUMINUM ALLOYS SECONDARY UNPROCESSED IN INGOTS IN THE FORM OF PIECES OF SIZE 695-645X70-100X45MM GRADE ADC12 ACCORDING TO STANDARD JIS H 5302-2006 WITH ULTIMATE TENSILE STRENGTH LESS THAN 216 MPa AT TEMPERATURE OF 298 K FOR USE IN METALLURGY | XXXXXXXXXX | 1 | N/A | 496974.11 | China | NINGBO |
3/6/2024 | 7601208002 | ALUMINUM ALLOYS, SECONDARY, UNPROCESSED, INGOTS, GRADE AK5M2, GOST 1583-93 (COMPOSITION: ALUMINUM 91.00-92.50%, COPPER 1.50-1.68%, MAGNESIUM 0.41-0.48%, SILICON 4.10-4.90%, IRON 0.51-0.91%, MANGANESE 0.21-0.28%, NICKEL 0.04-0.06%, ZINC 0.33-0.89%, TITANIU | XXXXXXXXXX | 1 | N/A | 37499.69 | Poland | GDANSK |
2/29/2024 | 7601208002 | ALUMINUM ALLOYS SECONDARY UNPROCESSED IN INGOTS IN THE FORM OF PIECES OF SIZE 695-645X70-100X45MM GRADE ADC12 ACCORDING TO STANDARD JIS H 5302-2006 WITH ULTIMATE TENSILE STRENGTH LESS THAN 216 MPa AT TEMPERATURE OF 298 K FOR USE IN METALLURGY | XXXXXXXXXX | 0 | N/A | 199997.66 | China | DALIAN |
2/29/2024 | 7601208002 | ALUMINUM ALLOYS SECONDARY UNPROCESSED IN INGOTS IN THE FORM OF PIECES SIZE 695-645X70-100X45MM GRADE ADC12 ACCORDING TO STANDARD JIS H 5302-2006 WITH ULTIMATE TENSILE STRENGTH LESS THAN 216 MPa AT TEMPERATURE OF 298K FOR USE IN METALLURGY | XXXXXXXXXX | 0 | N/A | 597909.51 | China | SHANGHAI |
2/21/2024 | 7601208002 | ALUMINUM ALLOY GRADE AK5M2 IN ACCORDANCE WITH GOST 1583-93, IN THE FORM OF 15-22.5 KG INGOTS, ARE MANUFACTURED BY THE TECHNOLOGY OF MELTING ALUMINUM-CONTAINING SCRAP AND WASTE. THE TENSILE STRENGTH OF ALLOYS AT A TEMPERATURE OF 298 °K (25 0C) IS LESS THAN 170 | XXXXXXXXXX | 0 | N/A | 3196013.69 | Turkey | NOVOROSSIYSK |
2/19/2024 | 7601208002 | SECONDARY ALUMINUM ALLOYS OF THE GRADE "AK9M2", IN THE FORM OF INGOTS IN BUNCHES, UNPROCESSED, THE TENSILE STRENGTH IS LESS THAN 205 MPa AT A TEMPERATURE OF 200 DEG C AND LESS THAN 398 MPa AT A TEMPERATURE OF 25 DEG C. | XXXXXXXXXX | 0 | N/A | 3348300.45 | China | USSURIYSK |
2/16/2024 | 7601208002 | SECONDARY ALUMINUM ALLOYS OF THE GRADE "AK9M2", IN THE FORM OF INGOTS IN BUNCHES, UNPROCESSED, THE TENSILE STRENGTH IS LESS THAN 205 MPa AT A TEMPERATURE OF 200 DEG C AND LESS THAN 398 MPa AT A TEMPERATURE OF 25 DEG C. | XXXXXXXXXX | 0 | N/A | 3091506 | China | DUNIN |
2/7/2024 | 7601208002 | SECONDARY ALUMINUM ALLOYS OF THE GRADE "AK9M2", IN THE FORM OF INGOTS IN BUNCHES, UNPROCESSED, THE TENSILE STRENGTH IS LESS THAN 205 MPa AT A TEMPERATURE OF 200 DEG C AND LESS THAN 398 MPa AT A TEMPERATURE OF 25 DEG C. | XXXXXXXXXX | 0 | N/A | 3024190.95 | China | DUNIN |